Joint fillers and floor repair products for warehouses, plants and distribution buildings

Colorado Concrete Repair installs Metzger/McGuire joint fillers and floor repair products in warehouses, plants and distribution buildings in the Denver metro. Forklift wheels break down joint edges until they spall. Our quotes name Metzger/McGuire products such as Armor-Hard repair epoxy, MM-80 and Edge-Pro 90 joint fillers and Spal-Pro Stabilizer foam. Metzger/McGuire sells through distributors. We do the prep, the repair and the install.

Clean warehouse aisle with a repaired concrete floor in service, racking and inventory on both sides
Repaired concrete floor in a warehouse aisle, back in service. Our install.

OR, TELL US ABOUT YOUR PROJECT:

Request a Site Assessment →

We Install Metzger/McGuire

Metzger/McGuire is one of four maker lines we install on a regular basis. Our joint and spall repair quotes name its products.

More Than 1,000 Jobs

We have done more than 1,000 jobs. That count is for our whole company.

Joint Repair in Our Quotes

Our warehouse joint quotes list steps such as cleaning out joints and cracks with a joint saw. The saw is attached to a HEPA vacuum. Then the quotes fill the joint and shave the filler flush.

JOINT FILLER AND REPAIR

Metzger/McGuire Products in Our Quotes

Metzger McGuire is specified when the problem is slab edge breakdown, failing joints, wheel-path abuse, or an uneven floor that disrupts operations. The right product depends on joint function, traffic type, cure timing, and whether the project also needs grinding, patching, or level correction.

RS 88

Fast Joint Filler for Operational Floors

Spal-Pro RS 88 is the maker’s rapid-set semi-rigid polyurea joint filler. Metzger/McGuire lists it for “trafficked industrial and retail concrete floors” and as “Ideal for Use in Stained/Polished Floors.” It says RS 88 “will not smudge or smear during grinding/polishing.” Our recent joint quotes name Edge-Pro 90 and MM-80.

MM-80

Semi-Rigid Protection for Saw-Cut and Construction Joints

MM-80 is the maker’s 5:1 semi-rigid epoxy joint filler. Metzger/McGuire lists it for floors “subject to hard wheeled material handling traffic and heavy loads.” Our quotes pair MM-80 with a sand-modified patch. On new concrete, its sheet says it “should not be installed prior to 30 days.”

LEVELING AND REPAIR

Floor Rehab for Trip Hazards and Wheel Impact

Many of our joint quotes cover more than filler. They list cutting around crushed areas, chipping out unsound concrete and patching back with Armor-Hard Concrete Repair Epoxy. Where it is needed, they add grinding along patches for smooth forklift pass-over. Where slabs rock, some quotes add Spal-Pro Stabilizer foam.

Why Joint Edges Keep Breaking Under Forklifts

Buyers name forklift wheels, most of all steel and hard rubber ones, as the cause of joint failure. Metzger/McGuire says softer fillers “deflect under loads, allowing joint edges to deteriorate (spall).” Its joint filler sheets also say “There are no government or ASTM standards for semi-rigid joint fillers.”

Surface preparation is 80-90 percent of the time we spend on a job. On joint work, our quotes list cleaning joints and cracks with a HEPA vacuum and wand before filling. Where a patch sits high, a quote adds diamond grinding with grinders attached to HEPA vacuums.

Access, phasing and off-hours work can be part of a quoted plan. We agree access and cure conditions for each job. The maker’s data sheet sets when a joint or patch can take forklift traffic.

Where Metzger McGuire Systems Fit Best

  • Distribution centers and warehouses with repeated forklift traffic over saw-cut and construction joints
  • Food and beverage facilities where damaged joints collect debris, disrupt sanitation, or create wheel-path failure
  • Manufacturing plants with hard wheel traffic, impact, and joint shoulder deterioration
  • Loading bays and service areas where edge breakdown becomes a safety and maintenance problem
  • Facilities preparing for polishing, sealing, or resinous flooring that need joints stabilized first
  • Operational buildings where level transitions and joint failure are creating ride-quality or trip-hazard issues

What CCR Reviews First

Joint Type

Saw-cut or construction

Traffic

Forklift and wheel load

Damage

Spalls and shoulder failure

Ride Quality

Flushness and flatness

Downtime

Return-to-service window

Metzger McGuire Systems Compared

Open a product to see what Metzger/McGuire lists for it and what our quotes name.

RS 88 Joint FillerPolyurea, rapid set▼

Where the maker lists it: “trafficked industrial and retail concrete floors,” and “Ideal for Use in Stained/Polished Floors,” per Metzger/McGuire.

What the maker lists:

  • Semi-rigid polyurea, mixed 1:1
  • Fill to full saw-cut depth
  • Slab at least 30 days old; ACI 60 to 90 days

Limits:

  • Our recent joint quotes name Edge-Pro 90 and MM-80
  • The maker warns of “bubbling and/or compromised adhesion” if moisture is excessive
  • Traffic times follow the maker’s data sheet
MM-80 Semi-Rigid Joint FillerEpoxy, heavy traffic joints▼

Where the maker lists it: Floors “subject to hard wheeled material handling traffic and heavy loads,” per Metzger/McGuire.

What the maker lists:

  • 5:1 semi-rigid epoxy joint filler
  • Full saw-cut depth, or 2 inches minimum where deeper
  • Service from 40°F to 120°F

Limits:

  • Not before 30 days on new concrete, per the maker
  • “ACI recommends a slab cure of 60-90 days or longer,” per the maker
  • Refrigerated floors need 7 to 14 more days, per the maker
Repair and Leveling SystemsArmor-Hard patching and Stabilizer foam▼

Best for: Delaminated, crushed or void areas that our quotes mark as a hazard to daily operations.

In our quotes:

  • Saw cuts around crushed areas, with blades attached to HEPA filter vacuums
  • Patch back with Armor-Hard Concrete Repair Epoxy
  • Spal-Pro Stabilizer foam where slabs rock

Limits:

  • Some quotes can only estimate the Armor-Hard quantity in advance
  • Cure and return to traffic follow the maker’s data sheet
  • Phasing and off-hours work can be part of the quoted plan

FREQUENTLY ASKED QUESTIONS

Metzger McGuire Installer Questions

Common planning questions for joint filler and operational floor repair work.

Why use a semi-rigid joint filler instead of a flexible sealant?

Semi-rigid fillers support slab edges in traffic-bearing joints. Flexible sealants are designed for movement and weather sealing, not for repeated hard-wheel impact in a warehouse or manufacturing floor. If the joint takes forklifts, the slab edge usually needs support.

How long should we wait before filling new joints?

Metzger/McGuire says MM-80 “should not be installed prior to 30 days” and that “ACI recommends a slab cure of 60-90 days or longer.” It lists 28 days minimum for Edge-Pro 90. Refrigerated floors need more time on its sheets. The sheet for the chosen filler sets the earliest fill date.

Do you grind the filler flush after installation?

Yes, when the joint takes wheel traffic. Our joint quotes list filling joints and cracks and shaving the filler flush. Where a patch or joint sits high, they add grinding for smooth pass-over of forklifts. The right finish depends on the filler, the traffic and the floor around the joint.

Can Metzger McGuire products be used in food or temperature-controlled facilities?

Yes. Metzger/McGuire makes Spal-Pro RSF as a “Joint Filler for Industrial and Freezer/Cooler Concrete Floors.” Our quotes include cooler-area void and joint repair, and freezer-space repair with Armor-Hard Extreme. The product has to match the room temperature, so the maker’s sheet decides which filler fits.

What if the concrete around the joint is already breaking apart?

Then the job is more than a filler install. Our quotes list cutting out crushed areas and patching back with Armor-Hard repair epoxy before the joint is filled. Metzger/McGuire lists Armor-Hard for “Spall repair/rebuilding of joint shoulders.” Some of our quotes say the Armor-Hard quantity can only be estimated in advance.

Need a Metzger McGuire installer for joints, wheel paths, or slab edge repair?

Give us a call. We install Metzger/McGuire joint fillers and repair products in Denver metro warehouses, plants and distribution buildings. Our quotes name Armor-Hard, MM-80, Edge-Pro 90 and Spal-Pro Stabilizer. We don’t do driveways or other house work, and pole barns are the one exception. We’ll set up a time to look.