Epoxy Floor Coating Problems: Warning Signs and What to Do Next
Epoxy Floor Problems in Denver: Peeling, Bubbles, Chips and What to Do Next
Colorado Concrete Repair repairs concrete floors and installs commercial epoxy flooring for commercial and industrial buildings in the Denver area. We don’t work on garage or basement floors. Pole barns are the one exception to our no house work line. Below, each problem shows its cause as a maker, one of our quotes or a buyer states it, and what our quotes list next.

Since 2009
Commercial and industrial floors in the Denver area.
More than 1,000 jobs
Our company-wide count across all our floor work.
18-grit or PCD tooling
What our quotes list to grind off failing paint or epoxy, on grinders attached to HEPA filter vacuums.
Common Epoxy Floor Problems and Their Causes
Open each one for the cause as its source states it and what our quotes list next.
Peeling or LiftingBond loss▼
What buyers see:The coating peels, flakes or lifts off the concrete. One food plant manager guessed that cleaning chemicals and water had weakened the bond.
✓ Causes the sources name:
- Moisture: Sherwin-Williams lists blistering and peeling of coatings among moisture problems
- Oil: one of our quotes said coatings on heavily oil-soaked concrete would be expected to fail
- Densifier: another quote said a densifier may act as a bond breaker for coatings
- Primer: one quote noted that MPE primer is not a moisture mitigation primer
What our quotes list next:
- Grind off the failing epoxy with PCD or diamond tooling on grinders attached to HEPA filter vacuums
- Vacuum the old coating remnants and dispose of them on site
- A moisture vapor barrier primer step to mitigate moisture related failure, when the scope includes it
For the full system and its prep, see our commercial epoxy flooring page.
Bubbles and BlistersMoisture▼
What buyers see:Raised bubbles or blisters in the coating. Buyers also describe coatings that break away from the concrete clean.
✓ Causes the sources name:
- Metzger/McGuire’s RS 88 sheet says it may bubble or lose adhesion if concrete or ambient moisture is excessive
- Sherwin-Williams ties moisture vapor to blistering and peeling of coatings
- Resinwerks names new, below-grade and no-vapor-retarder floors as high-moisture cases
- An engineer reported a new hangar floor at 89 to 94 percent RH against a 72 percent spec
What our quotes list next:
- Our quotes price floors at less than 3 lbs per 1,000 sq ft or less than 75% RH
- Above those limits, a moisture mitigation system may replace the primer by change order
- Resinwerks lists its Vapor Barrier Epoxy primer for damp concrete up to 99% RH
How we prep and install a floor: see our installation process.
Chips and Broken JointsForklift traffic▼
What buyers see:Chips at joints and in wheel paths. One engineer described joint failure from forklift wheels, especially steel and hard rubber wheels.
✓ What buyers and makers say:
- A shop owner wrote that forklifts aren’t friendly to epoxy unless they’re small with white tires
- Metzger/McGuire lists Armor-Hard epoxy mortar for spall repair and rebuilding joint shoulders
- Resinwerks lists its Epoxy Mortar Resurfacer for damaged or spalled floors
- Resinwerks lists its semi-rigid epoxy joint filler for saw-cuts in concrete floors
What our quotes list next:
- Prep, remove, fill and grind flush cracks, spalls and joints
- Construction joints honored where the scope says so
- Voids filled with Armor-Hard concrete repair epoxy
Systems we install for working floors: see our epoxy flooring systems.
Patches That Don’t MatchRepair or recoat▼
What buyers see:A patched floor that looks different from the rest. One of our repair quotes states that resinous patches with similar colors and flake blends will not match the existing failing floor.
✓ What our quotes list:
- Small failing areas repaired with resinous patches in similar colors and flake blends
- Some repair scopes quoted on time and materials
- Existing coating shaved off where adhered, with field shavers on HEPA vacuums
- Phased areas or off-hours work when the plan includes them
Limits:
- Patches will not match the existing failing floor
- A coating change can require a substantial recoat
- Cure time depends on the selected product and conditions
Topcoats in our quotes include Resinwerks polyaspartic systems.

EPOXY FLOOR PROBLEM QUESTIONS
Epoxy Floor Problems: Questions and Answers
Why is my epoxy floor peeling?
The sources name several causes. Sherwin-Williams lists blistering and peeling of coatings among moisture problems. One of our quotes said coatings on heavily oil-soaked concrete would be expected to fail. Another said a densifier may act as a bond breaker. One food plant manager guessed that cleaning chemicals and water had weakened the bond.
What causes bubbles or blisters in an epoxy floor?
Moisture is the cause the makers name. Metzger/McGuire’s RS 88 sheet says bubbling or lost adhesion may follow when concrete or ambient moisture is excessive. Sherwin-Williams ties moisture vapor to blistering. Our quotes price floors under set moisture limits, and a mitigation primer may be needed above them.
Can a failing epoxy floor be patched?
Sometimes, for small areas. One of our repair quotes lists resinous patches with similar colors and flake blends, and it states they will not match the existing failing floor. That scope was quoted on time and materials. If the coating itself has to change, that can mean a substantial recoat.
Does a failing epoxy floor have to come off?
When the floor is redone, our quotes list removing the failing epoxy first. They use PCD or diamond tooling on grinders attached to HEPA filter vacuums, then vacuum up the remnants. Where old coating is still bonded, one quote used field shavers on HEPA vacuums to shave it off where adhered.
Can the repair be phased around our operation?
It can be. Access, phasing and off-hours work can be part of a quoted plan. Phased areas or night work go in the quote when the plan includes them. Cure time depends on the selected product and conditions, so we agree access and cure conditions for the job.
Request a Site Assessment
If your floor is peeling, blistering or chipping, give us a call and we’ll set up a time to look at it.